Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.295 GPa @Temperature 120 °C |
42.8 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8253 HS PA6 (Dry) Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased.. |