Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 688 MPa

@Thickness 12.7 mm,
Temperature 427 °C
99800 psi

@Thickness 0.500 in,
Temperature 801 °F
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Tensile Strength, Ultimate 688 MPa

@Thickness 19.1 mm,
Temperature 371 °C
99800 psi

@Thickness 0.752 in,
Temperature 700 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..