Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 672 MPa

@Thickness 12.7 mm,
Temperature 371 °C
97500 psi

@Thickness 0.500 in,
Temperature 700 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Ultimate 672 MPa

@Thickness 3.20 mm,
Temperature 316 °C
97500 psi

@Thickness 0.126 in,
Temperature 601 °F
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..