Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 665 MPa

@Temperature 600 °C
96500 psi

@Temperature 1110 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..