Polymer Property : Tensile Strength, Ultimate = 91400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 630 MPa

@Temperature 550 °C
91400 psi

@Temperature 1020 °F
Solution Annealed prior to test
Special Metals INCONEL® Alloy HX
A nickel-chromium-iron-molybdenum alloy with outstanding strength and oxidation resistance at temperatures to 2200°F (1200°C). Matrix stiffening provided by the molybdenum content results in high..