Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 62.1 MPa @Temperature 649 °C |
9000 psi @Temperature 1200 °F |
SAE 1020 Steel sleeve joint |
Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. Due to the high flow point of this alloy, torch brazi.. |