Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 614 MPa @Temperature 204 °C |
89000 psi @Temperature 400 °F |
|
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability .. |