Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 827 MPa

@Temperature 21.1 °C
120000 psi

@Temperature 70.0 °F
Dry; ASTM D3039
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric
MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-..
Tensile Strength, Ultimate 827 MPa

@Thickness <=44.5 mm
120000 psi

@Thickness <=1.75 in
Crucible Steel Aquamet® 18 Stainless Steel
AQUAMET 18 is an austenitic stainless steel with corrosion resistance comparable to that of Type 304. Its good strength and toughness make it an ideal shafting material for workboats. It provides a ..
Tensile Strength, Ultimate 827 MPa

@Temperature 21.1 °C
120000 psi

@Temperature 70.0 °F
Crucible Steel XM-19 Stainless Steel
Crucible XM-19 Stainless is a nitrogen strengthened, low carbon, austenitic, stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosio..