Polymer Property : Tensile Strength, Ultimate = 791 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 791 MPa

@Thickness 12.7 mm,
Temperature 25.0 °C
115000 psi

@Thickness 0.500 in,
Temperature 77.0 °F
as welded
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Tensile Strength, Ultimate 791 MPa

@Thickness 9.50 mm,
Temperature 20.0 °C
115000 psi

@Thickness 0.374 in,
Temperature 68.0 °F
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..