Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 756 MPa @Thickness 9.50 - 25.4 mm, Temperature 316 °C |
110000 psi @Thickness 0.374 - 1.00 in, Temperature 601 °F |
|
Haynes Hastelloy® S alloy, flat products Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Ultimate | 756 MPa @Thickness 12.7 mm, Temperature 149 °C |
110000 psi @Thickness 0.500 in, Temperature 300 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Tensile Strength, Ultimate | 756 MPa @Thickness 12.7 mm, Temperature 149 °C |
110000 psi @Thickness 0.500 in, Temperature 300 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |