Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 726 MPa @Temperature 540 °C |
105000 psi @Temperature 1000 °F |
|
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |