Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 723 MPa

@Thickness 12.7 mm,
Temperature 204 °C
105000 psi

@Thickness 0.500 in,
Temperature 399 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Ultimate 723 MPa

@Diameter 12.7 mm,
Temperature 93.0 °C
105000 psi

@Diameter 0.500 in,
Temperature 199 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Ultimate 723 MPa

@Thickness 19.1 mm,
Temperature 204 °C
105000 psi

@Thickness 0.752 in,
Temperature 399 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..