Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 48.02 MPa @Temperature 100 °C, Time 2.42e+6 sec |
6965 psi @Temperature 212 °F, Time 672 hour |
Oven Aging |
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, high transparencyUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: VariousAvailable in.. |