Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 634 MPa @Thickness 23.4 mm, Temperature 400 °C |
92000 psi @Thickness 0.921 in, Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GMAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | 634 MPa @Thickness 46.1 mm, Temperature 400 °C |
92000 psi @Thickness 1.81 in, Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GMAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | 634 MPa @Thickness 25.4 mm |
92000 psi @Thickness 1.00 in |
Longitudinal Direction |
Alcoa 7055-T77511 Aluminum Extrusions Alcoa introduced alloy 7055 in the -T7751 temper for plate and the -T77511 for extrusions in 1991. This alloy was developed for use in compression-dominated structures (such as upper wing structures.. |