Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 593 MPa

@Thickness 12.7 mm,
Temperature 538 °C
86000 psi

@Thickness 0.500 in,
Temperature 1000 °F
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Ultimate 593 MPa

@Temperature 260 °C
86000 psi

@Temperature 500 °F
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel
INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability ..