Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 501 MPa

@Thickness 12.7 mm,
Temperature 538 °C
72700 psi

@Thickness 0.500 in,
Temperature 1000 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Tensile Strength, Ultimate 501 MPa

@Temperature 593 °C
72700 psi

@Temperature 1100 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Tensile Strength, Ultimate 501 MPa

@Temperature 593 °C
72700 psi

@Temperature 1100 °F
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..