Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 497 MPa @Temperature 760 °C |
72100 psi @Temperature 1400 °F |
AMS 5879 |
Haynes 625SQ® Nickel Alloy Sheet Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â.. |