Polymer Property : Tensile Strength, Ultimate = 43.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 43.4 MPa

@Temperature 260 °C
6300 psi

@Temperature 500 °F
ASTM D1708
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Direct Formed  (Unverified Data**)
Information provided by Daelim H&L