Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 400 MPa @Temperature 700.0 °C |
58000 psi @Temperature 1292 °F |
|
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel Description: DH2F is one of the best machining pre-hardened H13-type steels available.Unique Characteristics: 38-42 HRc hardness.Through hardened for exceptional dimensional stability.Cuts mold maki.. |
|||
Tensile Strength, Ultimate | 400 MPa @Temperature 316 °C |
58000 psi @Temperature 600 °F |
SAE 1020 Steel butt joint |
Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. Due to the high flow point of this alloy, torch brazi.. |