Polymer Property : Tensile Strength, Ultimate = 38.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 38.6 MPa

@Temperature 260 °C
5600 psi

@Temperature 500 °F
ASTM D1708
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Direct Formed  (Unverified Data**)
Information provided by Daelim H&L
Tensile Strength, Ultimate 38.6 MPa

@Temperature 260 °C
5600 psi

@Temperature 500 °F
ASTM D 638
Saint-Gobain Meldin® 2021 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..