Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 364 MPa @Temperature 93.0 °C |
52800 psi @Temperature 199 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 702 Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A.. |