Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 324 MPa @Thickness 50.83 - 76.2 mm |
47000 psi @Thickness 2.001 - 3.00 in |
|
Aleris Alustar H131 Aluminum Alloy Close in composition to AA5059. Used in defense and mining shielding applications for protection against ballistics and blasts. |
|||
Tensile Strength, Ultimate | 324 MPa @Thickness 50.83 - 76.2 mm |
47000 psi @Thickness 2.001 - 3.00 in |
|
Aleris Alustar H136 Aluminum Alloy Close in composition to AA5059. Used in defense and mining shielding applications for protection against ballistics and blasts. H136 has a higher elongation than H131 and so provides better protec.. |