Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 317 - 345 MPa @Temperature 22.2 °C |
46000 - 50000 psi @Temperature 72.0 °F |
Type 316 Stainless Steel butt joint |
Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. Due to the high flow point of this alloy, torch brazi.. |
|||
Tensile Strength, Ultimate | 317 MPa @Temperature 649 °C |
46000 psi @Temperature 1200 °F |
Vacuum |
ATI Wah Chang Nb/Nb Alloy C-103 This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig.. |