Polymer Property : Tensile Strength, Ultimate = 290000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2000 MPa

@Temperature 482 °C,
Time 10800 sec
290000 psi

@Temperature 900 °F,
Time 3.00 hour
Solution Annealed Plus Aged, AC
Special Metals UDIMAR® alloy 300 Fe-Ni Maraging Steel
UDIMAR® alloy 300 (UNS K93120) is an age-hardenable (maraging) iron-nickel steel combining ultra-high strength, toughness and resistance to crack propagation. The alloy is well suited to applica..