Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 185 MPa @Thickness 12.7 mm, Temperature 982 °C |
26800 psi @Thickness 0.500 in, Temperature 1800 °F |
As Welded, Solution Annealed, and Aged; Weld/Weld Fracture |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Ultimate | 185 MPa @Temperature 371 °C |
26800 psi @Temperature 700 °F |
|
Crucible Compaction Metals P/M Low Carbon Astroloy, Supersolvus P/M Low Carbon Astroloy is often the superalloy of choice when applications require greater ductility along with substantial strength levels. When HIP and heat treatment above the solvus temperatur.. |