Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 170 MPa

@Thickness 3.20 mm,
Temperature 982 °C
24700 psi

@Thickness 0.126 in,
Temperature 1800 °F
As Welded, Solution Annealed, and Aged; Base/Weld Fracture
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Tensile Strength, Ultimate 170 MPa

@Temperature 23.0 °C
24700 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-402 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 170 MPa

@Temperature 23.0 °C
24700 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 170 MPa

@Temperature 80.0 °C
24700 psi

@Temperature 176 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® TY-592GHV 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..