Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 240 MPa

@Temperature -40.0 °C
34800 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 1.6%); ASTM-D638
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 240 MPa

@Temperature 23.0 °C
34800 psi

@Temperature 73.4 °F
Crucible Compaction Metals Rene 95 Nickel Based Superalloy
P/M Rene 95 is one of the highest strength alloys available for service in the range of 800°F to 1200°F (425°C to 650°C). The alloy also provides excellent high temperature creep resistance and..