Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 235 MPa

@Temperature -40.0 °C
34100 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 1.7%); ASTM-D638
Toyobo GLAMIDE® T-602G30 MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 235 MPa

@Temperature -40.0 °C
34100 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-663G30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 235 MPa

@Temperature -40.0 °C
34100 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 1.75%); ASTM-D638
Toyobo GLAMIDE® T-665C30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..