Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 230 MPa @Temperature -40.0 °C |
33400 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 230 MPa @Temperature 23.0 °C |
33400 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 230 MPa @Temperature 23.0 °C |
33400 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 0.8%); ASTM-D638 |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 230 MPa @Temperature 23.0 °C |
33400 psi @Temperature 73.4 °F |
|
Crucible Compaction Metals Rene Supersolvus Rene 95 Nickel Based Superalloy Supersolvus P/M Rene 95 is designed to provide even higher temperature creep resistance and stress rupture strength than subsolvus Rene 95. Chemistry is not modified. These properties are obtained.. |
|||
Tensile Strength, Ultimate | 230 MPa @Temperature 204 °C |
33300 psi @Temperature 399 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 702 Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A.. |