Polymer Property : Tensile Strength, Ultimate = 22500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 155 MPa

@Temperature 760 °C
22500 psi

@Temperature 1400 °F
Crucible Compaction Metals P/M Low Carbon Astroloy, Supersolvus
P/M Low Carbon Astroloy is often the superalloy of choice when applications require greater ductility along with substantial strength levels. When HIP and heat treatment above the solvus temperatur..
Tensile Strength, Ultimate 155 MPa

@Temperature 980 °C
22500 psi

@Temperature 1800 °F
Haynes 617 Nickel Alloy Plate
Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed..