Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1610 MPa @Temperature 25.0 °C |
234000 psi @Temperature 77.0 °F |
|
International Mold Steel DH21 Die Cast & Forging Steel DH21 is for aluminum die cast dies.Information provided by International Mold Steel |