Tensile Strength, Ultimate 970 MPa

@Temperature 550 °C
141000 psi

@Temperature 1020 °F
Precipitation Hardened prior to test
Special Metals INCOLOY® Alloy 925
A precipitation-hardenable nickel-iron-chromium alloy with additions of molybdenum and copper. It combines the high strength of a precipitation-hardenable alloy with the excellent corrosion resista..
Tensile Strength, Ultimate 975 MPa

@Treatment Temp. 871 °C,
Time 3.60e+6 sec
141000 psi

@Treatment Temp. 1600 °F,
Time 1000 hour
Room temp test after thermal exposure
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..