Tensile Strength, Ultimate 89.6 MPa

@Temperature 482 °C
13000 psi

@Temperature 900 °F
Monel butt joint
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal
Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wet..
Tensile Strength, Ultimate 89.6 MPa

@Temperature 1370 °C
13000 psi

@Temperature 2500 °F
Vacuum
ATI Wah Chang Nb/Nb Alloy C-103
This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig..