Tensile Strength, Ultimate 1250 MPa

@Temperature 23.0 °C
181000 psi

@Temperature 73.4 °F
Special Metals INCONEL® Alloy X-750
A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with hig..
Tensile Strength, Ultimate 1250 MPa

@Temperature 23.0 °C
181000 psi

@Temperature 73.4 °F
Special Metals NIMONIC® Alloy 80A
A nickel-chromium alloy similar to NIMONIC alloy 75 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good corrosion and oxidation resistance and high tensile a..