Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 73.2 MPa @Temperature 23.0 °C |
10600 psi @Temperature 73.4 °F |
ASTM D1708 |
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Machined Parts Higher abrasion resistance than G15, high value stability and very low friction coefficient propertyInformation provided by Daelim H&L |