Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1045 MPa @Diameter 12.7 mm |
151600 psi @Diameter 0.500 in |
As Welded and Aged at 1850°F(1010°C)/2hr/AC + 1450°F(788°C)/8h/AC |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Ultimate | 1045 MPa @Temperature 23.0 °C |
151600 psi @Temperature 73.4 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 20% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |