Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Toughness | 0.0524 MPa | 7.60 psi | ASTM D790 |
CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic HYTAC-FLX has been improved for optimum performance in transparent applications. The enhanced formulation is easy to polish and results in minimal to no scratches with transparent sheet materials. .. |