Polymer Property : Flexural Toughness = 0.0800 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Toughness 0.0800 MPa
11.6 psi
CMT Materials HYTAC® B1X High Durability Thermoplastic Syntactic
HYTAC-B1X is the first plug assist material to combine the toughness of an engineered thermoplastic with the low thermal conductivity of syntactic foam. Plug assist made from HYTAC-B1X will resist ..