Mechanical Properties Metric English Comments
Flexural Toughness 0.0310 MPa
4.50 psi
ASTM D790
CMT Materials HYTAC® WFT High Temperature, Ultra-Smooth PTFE Impregnated
HYTAC-WFT combines the higher temperature, smooth surface properties of HYTAC-WF with PTFE impregnation for low stick surface capability and excellent material distribution. The result is a syntact..