Polymer Property : Peel Strength = 95.58 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength >= 16.75 kN/m
>= 95.58 pli
Typical
Parker Chomerics Tecknit Teckfip™ FIP-E Formed in Place Conductive Elastomer
Commercial grade FIP compound designed for moderate shielding performance. The Ag/glass particles are very smooth which leads to very low compression set value. The material is also available as a h..