Mechanical Properties Metric English Comments
Peel Strength 14.4 kN/m

@Temperature 23.0 °C
82.0 pli

@Temperature 73.4 °F
Aluminum, Bell Peel
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M