Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.09 - 14.0 kN/m | 6.20 - 80.0 pli | Average value: 5.21 kN/m Grade Count:38 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |