Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Peel Strength = 8.41 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 8.41 kN/m
48.0 pli
Aluminum
Momentive Performance Materials RTV5812 One-Component, Modified Alkoxy Adhesive Sealant, White
RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature...
Peel Strength 8.41 kN/m
48.0 pli
Aluminum
Momentive Performance Materials RTV5813 One-Component, Modified Alkoxy Adhesive Sealant, Black
RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature...
Peel Strength 8.41 kN/m
48.0 pli
Aluminum
Momentive Performance Materials RTV5818 One-Component, Modified Alkoxy Adhesive Sealant, Translucent
RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature...
Peel Strength 8.41 kN/m
48.0 pli
180°, Aluminum
3M Scotch-Weld™ TE230 Black Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Copyright © lookpolymers.com All Rights Reserved