Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 8.24 kN/m | 47.0 pli | |
Momentive Performance Materials RTV5812 One-Component, Modified Alkoxy Adhesive Sealant, White RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Peel Strength | 8.24 kN/m | 47.0 pli | |
Momentive Performance Materials RTV5813 One-Component, Modified Alkoxy Adhesive Sealant, Black RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Peel Strength | 8.24 kN/m | 47.0 pli | |
Momentive Performance Materials RTV5818 One-Component, Modified Alkoxy Adhesive Sealant, Translucent RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Peel Strength | 8.24 kN/m | 47.0 pli | 180°, Polyacrylic |
3M Scotch-Weld™ TE230 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 8.24 kN/m | 47.0 pli | 180°, ABS |
3M Scotch-Weld™ TE230 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |