Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.16 kN/m | 6.60 pli | Bond Strength (S2 to S2); Arlon SQA-TMS-011 |
Arlon 56866R026 0.028" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil LDPEThis data represents typical values for the production mater.. |