Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 6.49 kN/m | 37.0 pli | To anodized aluminum |
Momentive Performance Materials IS808 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, Translucent IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |
|||
Peel Strength | 6.49 kN/m | 37.0 pli | To anodized aluminum |
Momentive Performance Materials IS800.09 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, Aluminum IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |
|||
Peel Strength | 6.49 kN/m | 37.0 pli | To anodized aluminum |
Momentive Performance Materials IS802 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, White IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |
|||
Peel Strength | 6.49 kN/m | 37.0 pli | To anodized aluminum |
Momentive Performance Materials IS803 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, Black IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |
|||
Peel Strength | 6.49 kN/m | 37.0 pli | Lexan Polycarbonate® |
Momentive Performance Materials RTV6702 One-Component, Modified Alkoxy Adhesive Sealant, White RTV6700 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Peel Strength | 6.49 kN/m | 37.0 pli | Lexan Polycarbonate® |
Momentive Performance Materials RTV6703 One-Component, Modified Alkoxy Adhesive Sealant, Black RTV6700 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Peel Strength | 6.49 kN/m | 37.0 pli | Lexan Polycarbonate® |
Momentive Performance Materials RTV6708 One-Component, Modified Alkoxy Adhesive Sealant, Translucent RTV6700 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |