Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 6.14 kN/m | 35.0 pli | Tensile |
Dielectric Polymers NT-4511 High Temperature Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film. For applicati.. |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Tensile |
Dielectric Polymers NT-5513 High Tack Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film. For applicati.. |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Tensile |
Dielectric Polymers NT-9511-2 High Tack Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film. For applicati.. |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Tensile |
Dielectric Polymers NT-2802 Ultra Tack Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film at zero wet out.. |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Tensile |
Dielectric Polymers NT-2811 Ultra Tack Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film at zero wet out.. |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Tensile |
Dielectric Polymers NT-7411-5 Fume Mask
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Good conformabilityChemical resistantApplications: For protecting large areas of printed circuit boards from splash and fumes duri.. |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Tensile |
Dielectric Polymers NT-5511-2 Masking Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityHigh temperature resistantApplications: For automotive and other masking .. |
|||
Peel Strength | 6.14 - 7.01 kN/m | 35.0 - 40.0 pli | |
ITW Devcon Epoxy HP 250, Straw Information provided by ITW Devcon |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Glass |
Momentive Performance Materials N-Sil® RTV122 Silicone Modified Alkoxy Adhesive Sealants, White N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer.. |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Glass |
Momentive Performance Materials N-Sil® RTV128 Silicone Modified Alkoxy Adhesive Sealants, Translucent N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer.. |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Aluminum |
Momentive Performance Materials RTV6702 One-Component, Modified Alkoxy Adhesive Sealant, White RTV6700 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Aluminum |
Momentive Performance Materials RTV6703 One-Component, Modified Alkoxy Adhesive Sealant, Black RTV6700 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Aluminum |
Momentive Performance Materials RTV6708 One-Component, Modified Alkoxy Adhesive Sealant, Translucent RTV6700 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | T-peel |
Master Bond EP21TDCF-3 Two Component, Higher Viscosity Epoxy System Product Description: Master Bond EP21TDCF-3 is a two component epoxy for high performance bonding and sealing. It is formulated to cure rapidly at room temperature or faster at elevated temperatures.. |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Cure cycle: 3 days @ RT, with Acid Etched 6061-T6 Aluminum |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some.. |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | 180° |
3M Scotch-Weld™ DP-105 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s.. |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | PP, 180° |
3M Scotch-Weld™ 3748 VO Hot Melt Adhesive Self-extinguishing version of 3748 and Meets UL 1410 requirementsInformation provided by 3M |
|||
Peel Strength | 6.14 kN/m | 35.0 pli | Tensile |
Dielectric Polymers NT-511C High Temperature Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film. For applicati.. |