Mechanical Properties Metric English Comments
Peel Strength 10.408 kN/m
59.375 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7893 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These..
Peel Strength 10.408 kN/m
59.375 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7980 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These..