Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 9.90 kN/m | 56.5 pli | Al to Al, Honeycomb Climbing Drum Peel; ASTM D1781 |
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f.. |