Mechanical Properties Metric English Comments
Peel Strength 5.77 kN/m
32.9 pli
Valley Adhesives EM-421 High Temperature Application Glue Stick
Valley Adhesives EM-421 High Temperature Application Glue StickRapid strength build up; Excellent hot tacking and wetting; Bonds corrugated boxes and paper in packaging operations and repackaging ar..